i am also interested in vacuum desiccating after oxide instead of 
baking. someone please reply.
thank you.

andy white
-------------


From:    [log in to unmask] (keith larson)
To:      [log in to unmask]
cc:      
Date:    Fri, 30 Aug 96 13:20:57 -0500 (CDT)
Subject: RE: Vacuum Desiccating



FYI



>Return-Path: <[log in to unmask]>
>Received: by mail.airmail.net (/\##/\ Smail3.1.30.16 #30.74)
>	id <[log in to unmask]>; Fri, 30 Aug 96 10:56:25 -0500 (CDT)
>Received: from ipc.org by simon.ipc.org via SMTP
(940816.SGI.8.6.9/940406.SGI)
>	 id KAA16319; Fri, 30 Aug 1996 10:46:40 -0700
>Resent-Date: Fri, 30 Aug 1996 10:46:40 -0700
>Received: by ipc.org (Smail3.1.28.1 #2)
>	id m0uwVH8-0000QFC; Fri, 30 Aug 96 10:14 CDT
>Resent-Sender: [log in to unmask]
>Old-Return-Path: <[log in to unmask]>
>X400-Received: by /c=US/admd=MCI/prmd=Honeywell/; converted ( IA5-Text); 
>   Relayed; 30 Aug 1996 10:21:24 -0500
>X400-Received: by mta HW-MTA-AZ in /c=US/admd=MCI/prmd=Honeywell/; converted
(
>   IA5-Text);  Relayed; 30 Aug 1996 10:21:24 -0500
>X400-MTS-Identifier: [/c=US/admd=MCI/prmd=Honeywell/;
06638322706F452A-HW-MTA-AZ]
>Content-Identifier: 06638322706F452A
>Content-Return: Allowed
>X400-Content-Type: P2-1988 ( 22 )
>Conversion: Allowed
>Original-Encoded-Information-Types: IA5-Text
>Priority: normal
>Disclose-Recipients: Prohibited
>Alternate-Recipient: Allowed
>X400-Originator: [log in to unmask]
>X400-Recipients: non-disclosure;
>Message-Id: 
>
<06638322706F452A*/c=US/admd=MCI/prmd=Honeywell/o=AZ-MTA/ou=MSMail/ou=CAS/s=
Edwards/g=Ted/i=A/@MHS>
>Date: 30 Aug 1996 10:21:24 -0500
>From: "Edwards, Ted A (AZ75)" <[log in to unmask]>
>To: "[log in to unmask]" <[log in to unmask]> (Return requested)
>Subject: RE: Vacuum Desiccating
>MIME-Version: 1.0
>Resent-Message-ID: <"lpdfh3.0.qfE.6Lm9o"@ipc>
>Resent-From: [log in to unmask]
>X-Mailing-List: <[log in to unmask]> archive/latest/6031
>X-Loop: [log in to unmask]
>Precedence: list
>Resent-Sender: [log in to unmask]
>
>When we were in the board fabrication business, we did not store layers in a

>vacuum with desiccant but  when we used vacuum frame we would pull a vacuum 
>and hold it for more than 30 minutes before lamination.  When we switched to

>a vacuum lamination we continued to use a vacuum in the press and hold 
>before lamination.  We also pulled a vacuum on the prepreg and back filled 
>it's storage chamber with dry nitrogen.  The froth at the edge of the board 
>when down but we did not know if that was from the vacuum steps or the fact 
>we went to low pressure lamination when we switched to vacuum lamination.
> ----------
>From: [log in to unmask]
>To: [log in to unmask]
>Subject: Vacuum Desiccating
>Date: Friday, August 30, 1996 6:38AM
>
>Has anyone done testing, or incorporated as part of normal processing, the
>use of vacuum desiccating instead of baking after layer oxide coating, prior

>to
>lay-up and lamination. I would appreciate any information that is available.
>
>
>Bob G.
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To unsubscribe from this list at any time, send a message to:           *
>* [log in to unmask] with <subject: unsubscribe> and no text.        *
>***************************************************************************
>
>
>

andy white

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2