Thanks Gary, Genny, and Dave!
I wonder why I got Charles email all garbled like that? I get those every
once in a while...I was attributing it before to the email being sent using a
foreign language character set, obviously that wasn't the case if all of you
could read it...strange stuff?
Thanks again, and thank you Charles!
-Steve Gregory-
P.S. Charles, I would appreciate it if you would send me the info you
have...next week would be fine, and most appreciated! Also, I don't think
we have the same customer...
In a message dated 12/14/01 2:19:37 PM Central Standard Time,
[log in to unmask],
[log in to unmask], and [log in to unmask] writes:
> From: "Charles Caswell" <<A HREF="mailto:[log in to unmask]">[log in to unmask]</A>>
> Subject: Re: [TN] Alumina filled Polysulfide compound...
> Date: Friday, December 14, 2001 11:28 AM
>
> Steve, I am at home so I don't have the info here . We use the same stuff
> to bond components on some boards. I don't think you will find the stuff
> already mixed with the AlO2. I couldn't. The polysulfide IS fuel tank
> sealant. We mix it in small batches with approx. equal parts of AlO2 and
> the base material by weight. I wonder if we have the same customer. I will
> try to get into work tommorow and send some info, if not then on Mon. By
> the way, the stuff stinks.