TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Transfer-Encoding:
7bit
Sender:
Subject:
From:
Francis Lai <[log in to unmask]>
Date:
Wed, 15 Sep 1999 22:35:00 -0700
Content-Type:
text/plain; charset=us-ascii
MIME-Version:
1.0
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Francis Lai <[log in to unmask]>
Parts/Attachments:
text/plain (28 lines)
We are using pattern plating. After carbon treatment of our acid plating
bath, we ran dummies for 2 hours then plate our panels. However the area
around the holes showed dull and slightly rough finishes. The areas
which have no holes showed shiny. We use the plating bar method. We
etched the pattern and then use platting bar for connections. We ran two
panels in a bath which was not carbon treated and they were fine. The
PTH walls looked dull and slightly rough too. Can anyone help?

My e-mail : [log in to unmask]

Thanks!!!!!

Francis

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2