IPC-A-610 also requires a minimum end joint width, and a minimum
side joint length.
If the lead is not overhanging the side of the pad, you must
have a wetted fillet on both sides of the lead. The minimum
length of this side connection is different for Class 1 and Classes
2,3. If the lead overhangs the pad on one side, this
requirement only applies to the opposite side.
In 610D, this is on page 8-49, and in 610E, it's on page 8-55.
-Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Robert N
Sent: Tuesday, May 18, 2010 3:07 PM
To: [log in to unmask]
Subject: [TN] Acceptabe Solder Fillet on Gull wings
IPC 610 Cl 2 states that a side overhang of 50% is acceptable. Does that means, which seems obvious but not stated, that an acceptable solder fillet is required on one side only? Does the same apply to the toe, which allows for an overhang?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|