TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Juan T. Marugán" <[log in to unmask]>
Date:
Tue, 30 Sep 2008 13:17:50 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joe Russeau <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; format=flowed; charset="Windows-1252"; reply-type=original
From:
Joe Russeau <[log in to unmask]>
Parts/Attachments:
text/plain (73 lines)
Hi Juan,

You indicate that you see no issues with other suppliers of boards made from 
the same materials of construction.  Perhaps, therein lies an area to 
investigate. Maybe the supplier of the boards, where problem is arising, is 
not doing an adequate job of cleaning the boards before sending them to you. 
I don't recall you mentioning the final surface finish.  However, it could 
be possible that there are surface fabrication residues (ex. HASL flux 
residues) being left behind that when sent through your assembly operations 
are baked even more, which would make them harder to remove, especially with 
your current solvent process. Just a thought.

Best Regards,

Joe Russeau


----- Original Message ----- 
From: "Juan T. Marugán" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, September 30, 2008 12:19 PM
Subject: Re: [TN] Big problem when coating with Parylene C.


Well, we have now two problems, but I don't want to open a forum about the
expiration date for the use of 141-b.

Let me re-center the problem. Brian, I agree with you. We should be using
141-b MGX, but why we have obtained good results in other boards (diferent
P/N and different manufacturer, but polyimide boards also) conformal coated
at the same time that the other one? If we used the same solder paste, the
same cleaning solvent, the same outgassing, the same thermal cycling after
coating... the results should be the same.

One of the trials we did was cleaning a couple of boards with plasma. The
results were also bad.

For that reson we are looking for some incompatibility between Parylene C 
and
our polyimide laminate.

Is there anybody out there that experienced a problem of non-compatibility 
of
materials when coated a board with Parylene C?

Anyway, thank you Brian for your help.

Juan

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2