> Pratap, immersion tin coatings will loss their solderability in less than 24
> hours. You may be able to use very aggressive fluxes and solder to immersion
PRATTA ELECTRONIC MATERIALS INC. -MANCHESTER -N.H.
TEL: 603-6278488 FAX: 603-6278799
ARE NOW MARKETING A NEW TIN IMMERSION CALLED:"OMIKRON",
THE SOLDERABILITY IS PROVEN TO BE 1 YEAR.(PASSED TEST OF AGEING
4 HOURS AT 155c.
IT CREATS NO WHISKERS.
YISRAEL LESHMAN
OCTAVA MARKETING
ISRAEL