        Bev: I'm assuming you are referring to Mixed Flowing
Gas(MFG)testing.  These are accelerated corrosion stress tests to
predict field life of electronic assemblies and components in various
environments such as business office,light industrial,heavy industrial
etc. This is accomplished by introducing trace amounts(ppb range)of
corrosive gases into a chamber for a given amount of time.
They are fairly complicated test procedures to run and correlate data
to. Unless you plan on doing a lot of this type of testing I would
recommend you send it out to a service.
There are a variety of testing labs that can do this for you. We have
used IBM Endicott (607-755-0123).They have quite a bit of experience
is this type of testing and the ability to effectively correlate the
accelerated testing to real world applications.
In addition to the various Battelle tests there are a series of ASTM
ones also
available. Take a look at ASTM B827,I believe a newer ASTM standard
may be out
but I don't recall the number
                                                Regards
                                                        Michael
Barmuta
                                                        Staff
Engineer
                                                        Fluke
Electronics
                                                        Everett Wa.
                                                        425-356-6076

>On Fri, 12 Dec 1997 12:01:46 -0800 Bev Christian wrote:

> From: Bev Christian <[log in to unmask]>
> Date: Fri, 12 Dec 1997 12:01:46 -0800
> Subject: [TN] BATTELLE FLOWING GAS TEST
> To: [log in to unmask]
>
> 1) Does anyone know where I can buy a Battelle Flowing Gas Test
> apparatus?
> 2)  Does anyone know where I can buy this service?
>
> Bev Christian
> Nortel
> 613-967-5407
> FAX 613-967-5237
> [log in to unmask]
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################


ATOM RSS1 RSS2