TECHNET Archives

January 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Gervascio, Thomas" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Gervascio, Thomas
Date:
Wed, 11 Jan 2006 17:24:11 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
Hi Fellow Techies- 
I am trying to get current on hot bar/laser soldering. I've had
experience with the Panasonic Soft Beam. We have an appication where I
am looking to replace hand sodlering of QFPs and SOICs with an automated
process - I can't use mass reflow due to some material incompatability
issues. I've used a Farco pulsed hot bar soldering system in the late
1980s (yes I'm dating myself) and also a Hughes Hot Bar soldering
system. The major problem we had in the past was when we stencil printed
and reflow the solder, the resulting convex shape would cause the leads
of QFPs to skew off to one side prior to completing the hot bar
soldering. We used Raychem SolderQuik (a ribbon of solder with a
polyimide web ) to overcome that issue. What concerns and experiences
does anyone have to offer.
 
Thanks
Tom Gervascio
Senior Process Engineer
Sypris Electronics

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2