TECHNET Archives

April 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=UTF-8
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Ken Bloomquist <[log in to unmask]>, [log in to unmask]
Date:
Wed, 16 Apr 2008 20:02:29 -0500
Reply-To:
Donald Vischulis <[log in to unmask]>
Subject:
From:
Donald Vischulis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (47 lines)
Ken

One of the causes behind outgassing can be thin copper plating - .0005 inch or less.  Baking will mask the outgassing, but you may want to verify the thickness plated in the holes to make sure there are no reliability problems.

Don Vischulis

-----Original Message-----
>From: Ken Bloomquist <[log in to unmask]>
>Sent: Apr 16, 2008 1:32 PM
>To: [log in to unmask]
>Subject: Re: [TN] Out Gassing
>
>Hi Bob,
>
>Thanks for the great information and videos. I've heard about out gassing
>for more years than I'd like to admit but that's the first time I've seen
>it, Great Stuff!!!
>
>Jon suggested 125C for two hours as a corrective bake. In your article you
>mentioned bake but no specifics. Like I said in an earlier email, we can
>only go to 140F, will that do anything?
>
>Thanks again,
>
>KennyB
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2