I will 2nd that. I have experienced a lot of voiding issues when there
are VIPs on uBGAs as well as other BGAs. Often the VIPs are the same
size whether they are located in a uBGA pad or a larger say 25 mil BGA
pad and consequently, its impact is significant. I am trying to get the
design group to always plug and cap all VIPs so this does not become an
issue.
One work around is to use a 2 mil stencil and paste/reflow the side of
the board with this issue prior to populating any side of the board! The
2 mils of paste helps fill the VIPs as long as they are not too big.
Adding an additional reflow to a non-populated board should not be an
issue but needs to be verified.
Good luck,
- Joe
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Vladimir Igoshev
Sent: Friday, August 31, 2007 9:04 AM
To: [log in to unmask]
Subject: Re: [TN] vOID IN Micro BGA
The presence of vias in the pads causes it. Mind, though, that even such
large voids might not affect a long time reliability of the joints.
Regards,
Vladimir
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of shankar rao
Sent: Friday, August 31, 2007 11:49 AM
To: [log in to unmask]
Subject: [TN] vOID IN Micro BGA
Dear All,
We are getting Large voids in Micro BGA on someof the pads having
PTH/via (greater than 40% in dia) after reflow soldering in one of our
multi layer PCB. We are using ROHS paste and ROHS component. Can I know
what may be the reason for these voids
Regards
SHANKAR
K. Shankar Rao
---------------------------------
Unlimited freedom, unlimited storage. Get it now
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|