Dewey, Marion,
Hey, be easy on Werner our res expert on reliability.  If I knew half as
much German as he knows English I would be happy!   :)

regards,
Bev
Nortel Networks
> -----Original Message-----
> From: Marion A. Graybeal [SMTP:[log in to unmask]]
> Sent: Wednesday, July 28, 1999 11:44 AM
> To:   [log in to unmask]
> Subject:      Re: [TN] Freeze Spray and BGAs
>
> Werner,
>
> I see that you and Dan Quail attended the same school (potatoe).
>
> Marion Graybeal
> ----- Original Message -----
> From: Werner Engelmaier <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Wednesday, July 28, 1999 10:07 AM
> Subject: Re: [TN] Freeze Spray and BGAs
>
>
> >Hi Darrelt,
> >What happened to your BGA is pretty obvious. Just consider what is
> physically
> >happening when you hit iot with the freeze spray.
> >You hit the BGA with the freeze spry from the top, I am sure. This
> quickly
> >cools the top layer of the BGA, the rest of the BGA to a lesser degree.
> That
> >sets up differential thermal shrinking (the opposite of thermal expansion
> on
> >heating), which causes the BGA to warp like a potatoe chip with the top
> >surface being concave. This puts tremendous tensile stresses on the
> solder
> >joints, as well as on other parts in the BGA depending on construction.
> On
> >top of which, the PCB does not cool very much at all (the BGA shields it
> from
> >the freeze spray) and sets up shear stresses between the BGA and the PCB.
> >I would not at all be surprised if failure analysis shows fractured
> solder
> >joints. likely in combination of soldering pads ripped out of the polymer
> >matrix.
> >
> >Werner Engelmaier
> >Engelmaier Associates, L.C.
> >Electronic Packaging, Interconnection and Reliability Consulting
> >7 Jasmine Run
> >Ormond Beach, FL  32174  USA
> >Phone: 904-437-8747, Fax: 904-437-8737
> >E-mail: [log in to unmask], Website: www.engelmaier.com
> >
> >##############################################################
> >TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> >##############################################################
> >To subscribe/unsubscribe, send a message to [log in to unmask] with
> following
> text in
> >the body:
> >To subscribe:   SUBSCRIBE TECHNET <your full name>
> >To unsubscribe:   SIGNOFF TECHNET
> >##############################################################
> >Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> >information.
> >If you need assistance - contact Gayatri Sardeshpande at [log in to unmask]
> or
> >847-509-9700 ext.5365
> >##############################################################
> >
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2