You have other problem: may be your PWB Tg is not suitable for the application. Let me guess: it should be polyimide board and got changed to FR4 for lower cost?
--------------------------
Sent using BlackBerry
----- Original Message -----
From: Dale Hart [mailto:[log in to unmask]]
Sent: Monday, March 28, 2011 03:01 PM
To: [log in to unmask] <[log in to unmask]>
Subject: [TN] Solder joint height control
Thanks all for the responses.
The reason for my interest, we were having numerous units returned from the
field. Analysis revealed cracked solder joints on the board. It was learned
the units were occasionaly being subjected to a 20C per minute thermal cycle out
in the field. The field failure was also subsequently verified by lab testing.
The units are encapsulated for vibration protection so our thoughts were to get
as robust a solder joint as possible and make sure the CTE and modulus at the
temperature extremes were as benign as possible.
I remember when we had real components on the board (poke through) and the
module had to encapsulated with a hard polymer a buffer coating was applied
(possibly silicone) before encapsulation to help reduce the forces on the
components, is this technique still in packaging folks play book?
Dale Hart
UTC
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|