TECHNET Archives

April 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 25 Apr 2005 17:00:09 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Wenger, George M." <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Wenger, George M." <[log in to unmask]>
Parts/Attachments:
text/plain (136 lines)
Jason,

What does your component lead look like?  When the component pulls out of the solder fillet how much "pull" does it take?  can you quantify how strong it is?  What does the foot of your lead look like compared to the pad it was sodlered to?  Just looking at the pad I don't see anything that leads me to believe you have a problem.

Regards,
George
George M. Wenger
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059 (908) 546-4531 [log in to unmask]


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Stephen Gregory
Sent: Monday, April 25, 2005 4:34 PM
To: [log in to unmask]
Subject: Re: [TN] Solder reflow


Hi Jason!

I got the pictures you sent to me posted up on my web page for
everyone to take a look at. Go to: http://www.stevezeva.homestead.com
and look at "Swiss Cheese Solder, and Swiss Cheese Solder 2".

What it looks like to me is that either the component had contamination on
the leads and didn't allow the solder to wet, or that the solder wasn't
liquidous
long enough to form the metallurgical bond, or allow all the voids to work
themselves
out of the joint...I see a lot of voids in the solder.

Do you know what your peak temperature was during reflow, and how long did
it stay
above liquidous?

Kind regards,

-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX


|---------+---------------------------->
|         |           Jason            |
|         |           <jlarson@PACIFICI|
|         |           NSIGHT.COM>      |
|         |           Sent by: TechNet |
|         |           <[log in to unmask]>|
|         |                            |
|         |                            |
|         |           04/25/2005 02:38 |
|         |           PM               |
|         |           Please respond to|
|         |           TechNet E-Mail   |
|         |           Forum; Please    |
|         |           respond to Jason |
|         |                            |
|---------+---------------------------->
  >--------------------------------------------------------------------------------------------------------------|
  |                                                                                                              |
  |       To:       [log in to unmask]                                                                              |
  |       cc:                                                                                                    |
  |       Subject:  [TN] Solder reflow                                                                           |
  >--------------------------------------------------------------------------------------------------------------|




Good day,
investigation into solder reflow performance reveals components that pull
out of the solder fillet with no damage to the component and the fillet is
left intact as well. Solder that was under the component looks like swiss
cheese with multiple holes.
What part of the reflow is the likely cause, conveyor speed, pre-heat,
reflow heat, or cool down?

Thanks in advance for any help
Jason

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------




__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc.  It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone.  In such event, you should destroy the message and
kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.  
If you have received it in error, please notify the sender
immediately and delete the original.  Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2