TECHNET Archives

July 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 31 Jul 2013 14:19:04 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Rex Waygood <[log in to unmask]>
Message-ID:
Subject:
From:
Rex Waygood <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (158 lines)
I was taught that a random failure is one for which you don't know the
cause. The implication being that there is no such thing as a random
failure.
However pragmatically, I'd log all available data and wait for instance
2 :-) 

rex

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David D. Hillman
Sent: 31 July 2013 13:22
To: [log in to unmask]
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter

Hi Wayne - One of my mentors always stated " a single random failure
does not constitute a trend". It is sometimes hard to convince a
customer of that rationale.

Dave



From:   Wayne Thayer <[log in to unmask]>
To:     <[log in to unmask]>
Date:   07/31/2013 06:27 AM
Subject:        Re: [TN] Singular 30% Void and Oversize Ball Diameter
Sent by:        TechNet <[log in to unmask]>



In  a high quality operation, all failures are supposed to be rare
events. 
 If you don't look at these very carefully and treat them as precious,
they will quickly multiply and overwhelm you.

This means investigation, but as I presume you are pointing out, it
probably doesn't warrant a herculean effort with just one example.  But
it does mean pretty thorough documentation in case it happens again.

Wayne

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Kerr, Bryan (UK)
Sent: Wednesday, July 31, 2013 3:04 AM
To: [log in to unmask]
Subject: Re: [TN] Singular 30% Void and Oversize Ball Diameter

Hi Leland

Seems like a random event to me if you are running thousands of boards a
day. Even a minute trace of some volatile material on the ball or PEC
pad could cause this. Perhaps not worth losing sleep over and put it in
the memory banks !

Regards


Bryan Kerr
Principal Quality Engineer
CMA Lab and Process Engineering
BAE Systems Maritime Services
Manufacturing Hillend
Hillend Industrial Estate
Hillend
Nr Dunfermline
Fife
Scotland
KY11 9HQ
01383-836097


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: 30 July 2013 19:18
To: [log in to unmask]
Subject: [TN] Singular 30% Void and Oversize Ball Diameter

----------------------! WARNING ! ---------------------- This message
originates from outside our organisation, either from an external
partner or from the internet.
Keep this in mind if you answer this message.
Follow the 'Report Suspicious Emails' link on IT matters for
instructions on reporting suspicious email messages.
--------------------------------------------------------

Folks,

We run thousands of boards a day, and almost every one carries a BGA.
We inspect each with inline X-ray.

Last week, we had one single ball to fail for a 30% void and an oversize
diameter.  We contacted the supplier, and they said their process was
incapable of sending out such a defect.

We've never had a void over 5%, and even those are incredibly rare.

What within our process might have caused this, and do you agree with
the statement of the supplier?  How do you recommend we analyze the
failure?

Thanks in advance for your help!

Leland

________________________________

?Confidentiality Notice:
This transmission (including any attachments) may contain confidential
information belonging to the sender and is intended only for the use of
the party or entity to which it is addressed. If you are not the
intended recipient, you are hereby notified that any disclosure,
copying, distribution, retention or the taking of action in reliance on
the contents of this transmission is strictly prohibited. If you have
received this transmission in error, please immediately notify the
sender and erase all information and attachments.?

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud
service.
For more information please contact helpdesk at x2960 or
[log in to unmask] 
______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2