TECHNET Archives

1996

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vJOlH-0000T3C; Fri, 1 Nov 96 12:56 CST
Old-Return-Path:
Date:
1 Nov 1996 10:42:25 -0800
Precedence:
list
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/7330
TO:
Return-Path:
<TechNet-request>
From [log in to unmask] Mon Nov 4 10:
01:10 1996
Resent-Message-ID:
<"k2bSP1.0.QSC.5VaUo"@ipc>
Subject:
From:
"Rex Breunsbach" <[log in to unmask]>
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (52 lines)
        Reply to:   RE>Wave Solder SPC
In terms of prevention, there are a couple good wave soldering process
monitoring tools on the market.  The WaveRIDER from ECD and the Wave Optomizer
from TIC.

--------------------------------------
Date: 10/31/96 9:13 PM
To: Rex Breunsbach
From: Kenny Bloomquist
We are trying to do SPC on our wave soldering process.  It seems that
everyone in our company has their own opinion as to what should be tracked.

I would like to hear from anyone who is successfully, (or unsuccessfully),
using SPC on their wave solder process and what it is that you are
measuring.  Some suggestions from our SPC group are as follows:

Prevention:  What do others "look at" and why?  Solder density, wave height,
various temperatures, angles, rates, etc.  How much impact does board
configuration have?  Tightly packed and complex or loose and simple? 

Failure:  What is a good measure of defects?  Defects per solder joint, per
hole, top and bottom, per board, per square inch, per component, per run,
per day, per XX minutes of run time, per ??

What questions should we be asking?  We still have boards that require
touch-up after wave solder, is there anyone who has eliminated that need in
the DOD and space application world?

Thanks in advance to all that respond.

Ken Bloomquist
Sr. Staff Process Eng.


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************



ATOM RSS1 RSS2