On Wed, 21 Feb 1996, Steve Quinn wrote:

>         We are wondering what is the latest rev of this spec(IPC-A-600D).
> We have one dated 9-25-89.  Specifically we are questioning allowable
> plating voids in through holes.  Are circumferential voids acceptable in
> current spec?  
> 

The latest revision of the IPC-A-600 is revision E which was published 
August 1995. Circumferential voids in excess of 90degrees are 
nonconforming for all three classes in the copper plating section. 


****************************************************
Jon Holmen
Technical Project Manager
IPC
2215 Sanders Road
Northbrook IL  60062-6135
Phone (847) 509-9700 ex329
Fax   (847) 509-9798
e-mail  [log in to unmask]
URL:http://www.ipc.org
*****************************************************



ATOM RSS1 RSS2