TECHNET Archives

September 2002

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Carl VanWormer <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Wed, 18 Sep 2002 08:43:35 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
We are planning to use an AGP-Pro connector (and a mating
card-edge connection on a add-in card) in a new design.
The AGP spec has the following information about plating
the contacts of the add-in card.

---------- Expansion Card Description
----------------------------------------
5.2.2 Contact Design
A requirement of 100 microinches (min) tin lead over nickel
underplate on solder tails, for all plating alternatives.
The following two plating alternatives are listed to allow
flexibility to connector suppliers. The absolute requirement
is that the plating must meet the qualification requirements
listed in Section 5.10.

Alternative 1: High strength copper alloy; 15 microinches
(min) gold plating over 50 microinches minimum nickel
plating.

Alternative 2: High strength copper alloy, 2 microinches
(min) gold flash over 15 microinches palladium-nickel
over 50 microinches (min) nickel underplate in critical
contact areas.
----------------------------------------------------------------------------
---

We are ignorant of some of the details of plating, so we can't
tell if this means a total of 3 alternatives (one tin-lead,
the other two with gold and stuff), or just 2 alternatives,
both being gold and stuff over the tin-lead.

Questions:

1.  How many alternatives are there (2 or 3)
2.  If gold is an option, what could we expect to pay (extra)
    for gold plating on an AGP card-edge connector?
3.  Is gold required for long term connection reliability?
4.  Is there a requirement for the plating on the board to
    match the plating on the connector?
5.  Are there any other questions I should be asking to stay
    out of trouble?

Thanks,
Carl



Carl Van Wormer
Cipher Systems (Day Job)
Testec (home of the ShortSniffer short circuit finder)
www.testecvw.com

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2