TECHNET Archives

February 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jean-François Bissonnette <[log in to unmask]>
Date:
Wed, 25 Feb 2009 13:13:03 -0600
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Douglas Pauls <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (194 lines)
Jean-Francois,
You are welcome.  You may also find the following narrative useful.  I 
wrote it as part of the revision of the IPC-HDBK-830, currently underway.

Doug Pauls
Rockwell Collins


Relation of IPC-CC-830 and MIL-I-46058 to Performance Specifications

Many individuals do not understand the relationship or nature of 
IPC-CC-830 or MIL-I-46058 to performance specifications, such as J-STD-001 
or IPC-A-610. 

IPC-CC-830 and MIL-I-46058 are both material qualification specifications. 
 The two documents are virtually identical.  Both of these documents 
specify a series of tests for conformal coating materials, on standard 
substrates, with defined minimum acceptability criteria.  The tests 
specified in these documents are those chosen by the military and 
high-performance segment of the electronics industry to examine the most 
critical elements of conformal coatings.

Passing these tests are no guarantee that the conformal coating will work 
in any given application and does not assure that the coating is ?good?. 
Nor does it mean that not qualifying to this specification indicates that 
the coating is ?bad?.  These two specifications merely set a minimum set 
of criteria for a coating to be considered for military or 
high-performance application.  The onus is, and has always been, on the 
OEM to determine if a coating is adequate for the end item application for 
the end use environment. 

The proper use of these two standards is for material selection, not 
material performance.  Example:  Conformal coating shall be qualified to 
MIL-I-46058, Type AR.

It is left to performance standards, such J-STD-001, or to individual 
customer requirements to define performance requirements for conformal 
coating on electronic assemblies. 




Jean-François Bissonnette <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
02/25/2009 10:51 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jean-François Bissonnette              <[log in to unmask]>


To
[log in to unmask]
cc

Subject
Re: [TN] IPC-CC-830






This may come a little late but thank you all for your answers. 

 

Jean-François Bissonnette

t : 450-967-7100 ext : 242

[log in to unmask]

www.digico.cc <http://www.digico.cc/> 

________________________________

De : [log in to unmask] [mailto:[log in to unmask]] 
Envoyé : 13 février 2009 18:02
À : TechNet E-Mail Forum; Jean-François Bissonnette
Objet : Re: [TN] IPC-CC-830

 


Jean-Francois, 

IPC-CC-830 is a materials qualification document, not a application or 
performance specification.  It sets the minimum criteria for coatings to 
be used in high performance electronics. 

IPC-A-610 and IPC-J-STD-001 both have coating sections, but both defer to 
the engineering drawing or print.  Essentially, the coating goes where the 
drawing says and coating does not go where the drawing specifies a keep 
out zone.  Required clearance depends on the drawing and the quality 
system of the customer. 

Doug Pauls
Rockwell Collins 



Jean-François Bissonnette <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]> 

02/13/2009 03:38 PM 

Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Jean-François Bissonnette              <[log in to unmask]>

To

[log in to unmask] 

cc

 

Subject

[TN] IPC-CC-830

 

 

 




Hi Technetters,



Can anyone tell me if there is a spec on the coverage of conformal 
coating, more precisely is there a required clearance on the edges of the 
PCBs?



Jean-François Bissonnette

Technologue - Documentation de procédés

t : 450-967-7100 ext : 242

Mtl : 514-990-5762

f : 450-967-7444




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2