TECHNET Archives

July 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Martin Butcher <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Martin Butcher <[log in to unmask]>
Date:
Thu, 20 Jul 2006 10:19:32 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (76 lines)
I've seen clamp/pallets that are spring loaded to make solid contact with
the pads and balls.

Best of luck,
Martin Butcher
Process Engineer

-----Original Message-----
From: Macko, Joe @ IEC [mailto:[log in to unmask]]
Sent: Thursday, July 20, 2006 10:16 AM
To: [log in to unmask]
Subject: [TN] temporary attachment of a BGA to a PCB for test


Fellow techs,



I have been asked to determine if there is a way to temporarily install a
BGA onto a test board using some type of conductive adhesive to make
electrical contact, electrical test and then safely remove the adhesive
without damaging the solder balls and be able to use the BGA.



Sounds impossible but I informed the design group I would check out the
options.



The other option we are looking at is to design a clamp/pallet that will
securely hold the BGA to the board.  The problem here may be making 100%
electrical contact on all 48 balls.



Anyone have any creative ideas they would like to share? Test sockets are
not an option.





thanks

Joe






---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2