TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 17 Jul 2009 10:31:29 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Mike Sewell <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Mike Sewell <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
Maybe not a film but Henkel has Macromelt...a "polymide hot melt
adhesive designed as a viable solution to encapsulate printed crcuit
boards (PCB). Applications include small circuit boards for consumer
electronics" 

Regards,
Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, July 17, 2009 9:53 AM
To: [log in to unmask]
Subject: [TN] Shrink Wrap a Board

Good morning all,

Now that we have thoroughly established most of us are ugly and don't
want 
our pictures bandied about, I have a question.  And Friday seems to be a

time for silly questions, so here goes.

Have any of you ever seen a product that essentially vacuum forms a 
plastic film over the surface of an assembly?  Not a chemical vapor 
deposition like Parylene or conformal coat process.  For a particular 
(really odd) application, I want to put a rain guard on the surface of
an 
assembly.  Something where I could take a squirt gun and shoot water at 
the assembly and never have it hit the surface (of the assembly). 

Don't ask why.

Doug Pauls

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2