TECHNET Archives

September 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
Doug Black <[log in to unmask]>
Date:
Thu, 23 Sep 1999 09:06:00 +0100
MIME-Version:
1.0
X-To:
"Taheri, Kamran" <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Doug Black <[log in to unmask]>
Parts/Attachments:
text/plain (53 lines)
We currently half cut our fiducials with our Laser's and gain a black enough
contrast that there is no need for these to be filled with black adhesive
after cutting. They stay black through all cleaning process's.

Doug Black
Technical  Manager
Dek Precsion Screens Division
Weymouth,England
Tel: (01305) 760909
[log in to unmask]
 ----------
From: Taheri, Kamran
To: [log in to unmask]
Subject: [TN] Fiducials
Date: 22 September 1999 21:28

Is there any other methods of putting fiducials on the stencil? Our vender
Laser cuts the fiducials half the thickness of the stencil then fills it
with black adhesive. After a while the black adhesive starts to deteriorate
and my phone rings of the hook. I usually get good results filling the
fiducials on the thicker stencils with Loctite 410 black adhesive. But not
much luck when dealing with 5 or 6 mils thick stencils. Any comments
appreciated.

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2