TECHNET Archives

July 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 30 Jul 2009 10:21:21 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
Jason Roetz <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (63 lines)
Shawn, 

You may want to consider simply making the vias a larger diameter,
rather than increasing the plating. If there's room for the larger vias,
I think this would be an easier option.

Regards,

Jason Roetz, CID+
Master Designer 
Eaton Corporation
Electrical Group, Industrial Controls Division
4201 North 27th Street 
Milwaukee, WI. 53216 
Telephone: 414-449-6397
Fax:  414-449-7319
[log in to unmask]
www.eaton.com


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Upton, Shawn
Sent: Thursday, July 30, 2009 9:06 AM
To: [log in to unmask]
Subject: [TN] Via plating question

Quick question: I usually have via's plated to a minimum of 1mil.  I
have a high current design where I'd like to have those via's plated to
2mil (near 2oz, to match the 2oz spec for the layers) -- but the board
has some 15mil vias and is a 125mil thick board.  Would a typical board
house be ok with this?  I don't care about getting those 15mil mil
diameter via's to 2mil barrel plating, only the 32mil ones need to be
that thick.

Shawn Upton, KB1CKT
Test Engineer
Allegro MicroSystems, Inc
[log in to unmask]
603.626.2429/fax: 603.641.5336

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2