The ageing effect of some dielectrics is large. It is quoted as percent
per LDR. Figures can be as high as 7% per LDR. (-7% hour 1, -7% next 10
hours etc) Reset is achieved by high temperature (Curie Point?) such as
soldering. So I've seen ICT fails for being too high when tested quickly
after reflow.
Close reading of some chip capacitor specs leads one to believe that
-100% plus infinity on tolerance is a valid spec.
I would look carefully at the spec of the capacitor designed in and
discuss with the board designer what is needed. It is quite possible
that the designer is unaware of the lack of stability in some
dielectrics.
Rex
Rex Waygood
Technical Manager
PartnerTech Poole Ltd
Benson Road
Poole
Dorset BH17 0RY
United Kingdom
Tel: +44 (0)1202 674333
Fax: +44 (0)1202 678028
DDI: +44 (0)1202 338222
Mob: +44 (0)7887 997403
[log in to unmask]
www.PartnerTech.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Ioan Tempea
Sent: 01 July 2008 16:18
To: [log in to unmask]
Subject: Re: [TN] Ceramic Cap Value
Hi Ken,
We've seen this phenomenon twice in the past 4 months, high rate of ICT
failure on ceramic caps and had the same issue, replacing the parts
sometimes worked and sometimes didn't. We even have a painful open case
on this matter.
I need more clarifications from the group regarding this issue and how
to get around it.
The paper on aging asks to take the phenomenon into account when
designing the circuitry.
Does this mean the high failure rate Ken and I witnessed is borderline
design?
Can it be marginal testing method also?
Can it be anything else that design or testing?
Thanks,
Ioan
-------------------------------------------------------------------------------
The information contained within this e-mail and any attachments contained therein may be confidential and/or legally privileged and is for the use of the intended recipient only. If you are not the intended recipient please delete it from your system and notify the sender by return e-mail. The content of this e-mail may not be copied or disclosed to any third parties without prior permission from the sender.
E-mail is susceptible to data corruption, interception, tampering and viruses. We do not accept any liability for any such incidents or any consequences thereof.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|