TECHNET Archives

June 2013

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Leland Woodall <[log in to unmask]>
Date:
Thu, 13 Jun 2013 14:30:56 +0000
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Stadem, Richard D." <[log in to unmask]>
Message-ID:
Subject:
From:
"Stadem, Richard D." <[log in to unmask]>
MIME-Version:
1.0
In-Reply-To:
Content-Transfer-Encoding:
base64
Content-Type:
text/plain; charset="utf-8"
Parts/Attachments:
text/plain (1 lines)
Try performing EDX on a bar of solder. 
Another question, if the trace amounts do not violate J-STD-006, then who cares?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Leland Woodall
Sent: Thursday, June 13, 2013 9:25 AM
To: [log in to unmask]
Subject: Re: [TN] Titanium

Just blind guessing on my part.  I was suspecting cross-contamination of some sort.  We utilize titanium wave soldering pallets, but they are cleaned in a dedicated machine.

I've never seen any trace of titanium during EDX analysis of our solder joints.

Leland

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Thursday, June 13, 2013 10:16 AM
To: [log in to unmask]
Subject: Re: [TN] Titanium

Richard, so What would cause it to leach into the solder? --  Improper coating application? Temperature of the solder in the pot?...etc., etc.,. would this show up in solder analysis? (Are the labs doing these analysis even checking for Ti?)

Leland, no Ti pallets on our products, but not sure if they are used on someone else's. I will check. However, is your concern that the Ti is leaching from the pallets into the saponifier and is being re-deposited on the assemblies in the wash?

Thanks,
Amol


-----Original Message-----
From: Stadem, Richard D. [mailto:[log in to unmask]]
Sent: Thursday, June 13, 2013 9:09 AM
To: TechNet E-Mail Forum; Amol Kane
Subject: RE: Titanium

Many newer wave-solder and selective solder machines have a titanium-lined pot and/or sump. The newer the machine, the higher the Ti count.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Amol Kane
Sent: Thursday, June 13, 2013 9:04 AM
To: [log in to unmask]
Subject: [TN] Titanium

Dear Technetters,
We are seeing some titanium residues (confirmed by EDX) on solder joints after wave soldering post wash (that is not to say they are not present post wave, more analysis is ongoing). Water soluble process, high lead alloy, and a saponified wash. So far the Ti residues are only detectable on the solder joints, not on the assy surface. For general information. what are some possible sources of Ti on the assembly?

Regards,
Amol



______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

________________________________

“Confidentiality Notice:
This transmission (including any attachments) may contain confidential information belonging to the sender and is intended only for the use of the party or entity to which it is addressed. If you are not the intended recipient, you are hereby notified that any disclosure, copying, distribution, retention or the taking of action in reliance on the contents of this transmission is strictly prohibited. If you have received this transmission in error, please immediately notify the sender and erase all information and attachments.”

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2