TECHNET Archives

April 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
X-To:
Date:
Mon, 6 Apr 1998 08:56:14 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Robisan1 <[log in to unmask]>
Content-type:
text/plain; charset=US-ASCII
Subject:
From:
Robisan1 <[log in to unmask]>
Content-transfer-encoding:
7bit
Parts/Attachments:
text/plain (32 lines)
In a message dated 98-04-03 15:41:04 EST, you write:

<< f we get readings in NaCl equiv., we still do not have this kind of
 separation, so SIR may not be of any value in answering this question.

 Jon  >>

SIR is the only thing that is going to tell you if the contaminants left
on the board will result in a decrease in insulation resistance or
electromigration.  It is a functional test - has a bias and humidity.
If contaminants are on the board between the combs then you will
see their effect.

The only problem is that in actual production, the contamination is
rarely dispersed over the entire board evenly.  It is usually trapped
between the lands of the most difficult part to clean under and around.

Susan Mansilla
Robisan Laboratory

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2