                Agreed.  I didn't mention crack initialization, due to
the fact we discovered that this generally only happened when personnel
left the assembled product in the cleaner for a long period of time.  (1
hour plus.)

                Cobey

                                -----Original Message-----
                                From:   Joy, Stephen C
[SMTP:[log in to unmask]]
                                Sent:   Wednesday, June 17, 1998 10:34
AM
                                To:     [log in to unmask]
                                Subject:        Re: [TN] Ultrasonic
cleaning

                        I have seen issues with crack initiation in
assembled solder joints in some
                        cases. Ultrasonic cleaning after x section
cutting has been statistically
                        confirmed as the culprit.
                        What you may be seeing are Ni oxidation effects.
                        Maybe the ultrasonic cleaner is a potential
process control tool!
                        Steve



                        In my experience, the only problems observed
with this
                        cleaning method is getting a cleaning solution
that will not leave a
                        nasty residue.  If rinsed and dried properly, we
have no defects.

                        Cobey Schmidt
                        VisionTek
                        1175 lakeside Drive
                        Gurnee, IL 60031
                        [log in to unmask]
                        <mailto:[log in to unmask]>
                        (847) 360-7566 voice
                        (847) 360-7443 fax

                        -----Original Message-----
                        From:   Modular Components National,
                        Inc. [SMTP:[log in to unmask]]
                        Sent:   Wednesday, June 17, 1998 9:19 AM To:
[log in to unmask]
                        Subject:        [TN] Ultrasonic cleaning

                        To all:
                        Are there any negative effects to using
ultrasonic cleaning on nickel/gold
                        plating?
                        My reason for asking is this.  We recently
plated two panels and tape
                        tested them prior to ultrasonic cleaning.  Then
after ultrasonic cleaning
                        and during our final machining process, we
experienced poor gold to nickel
                        adhesion.
                        Any input would be greatly appreciated.
                        Regards
                        Ryan
                        Modular Components National, Inc.
                        2302 Industry Court
                        Forest Hill, MD 2150
                        PH (410) 879-6553
                        Fax (410) 838-7629



################################################################
                                                TechNet E-Mail Forum
provided as a free service
                        by IPC using LISTSERV 1.8c


################################################################
                                                To
subscribe/unsubscribe, send a message to
                        [log in to unmask] with following text in the
body:
                                                To subscribe:
SUBSCRIBE TechNet <your full
                        name>
                                                To unsubscribe:
SIGNOFF TechNet


################################################################
                                                Please visit IPC web
site
                        (http://jefry.ipc.org/forum.htm) for additional
information.
                                                For technical support
contact Hugo Scaramuzza at
                        [log in to unmask] or 847-509-9700 ext.312


################################################################


################################################################
                        TechNet E-Mail Forum provided as a free service
by IPC using LISTSERV 1.8c

################################################################
                        To subscribe/unsubscribe, send a message to
[log in to unmask] with following
                        text
                        in the body:
                        To subscribe:   SUBSCRIBE TechNet <your full
name>
                        To unsubscribe:   SIGNOFF TechNet

################################################################
                        Please visit IPC web site
(http://jefry.ipc.org/forum.htm) for additional
                        information.
                        For technical support contact Hugo Scaramuzza at
[log in to unmask] or
                        847-509-9700
                        ext.312

################################################################


################################################################
                        TechNet E-Mail Forum provided as a free service
by IPC using LISTSERV 1.8c

################################################################
                        To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
                        To subscribe:   SUBSCRIBE TechNet <your full
name>
                        To unsubscribe:   SIGNOFF TechNet

################################################################
                        Please visit IPC web site
(http://jefry.ipc.org/forum.htm) for additional information.
                        For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312

################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2