hi,

yes, i've been getting a lot of them, but not here at work.  in my case, my isp (att) tells me that this is a very troublesome problem.  you get these messages, even though you haven't sent them, because that's the way the worm works.  my pc is free of viruses, and you probably aren't infected either.  the only thing you can do is grin and bear it until the worm is eradicated on the net.  you should let your isp know you have this problem.

phil

-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Tuesday, September 09, 2003 7:46 AM
To: [log in to unmask]
Subject: [TN] Notices


Hi,
Are you all getting all these "failure notice", "Returned mail",
"Undeliverable message returned to sender", etc. about e-mails I have never sent to
addresses I have never heard of? This started about 4 or 5 days ago.

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2