We are performing solderabity tests using SERA method . You can test the
panels and not only the specimen . Contact the manufacturer , ECI at
[log in to unmask] .
Regards
At 19:59 20/10/98 -0400, you wrote:
>Hello to all the people in this list. I hope you can help me.
>
>1. Now that the direction the industry is taking is towards the
>development of packages with reduced lead widths (primarily because of
>the shrinking package size), is the "Dip and Look" method still the
>preferred test for Solderability Test?
>
>2. I have asked around other assembly companies and those who purchased
>the Wetting Balance system told me that they are unable to qualify the
>machine because of "calibration problems" and never got to use it since
>it was purchased. Do we have somebody here who encountered similar
>problems? Was it ever resolved? How?
>
>If there are suppliers of various Solderability Testers here, kindly
>e-mail me privately ([log in to unmask]). Thanks a lot.
>Best Regards,
>
>
>
>Lei Tumibay
>Lead Finish Group - Assembly Engineering
>Analog Devices - General Trias
>Cavite, Philippines
>E-mail: [log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|