TECHNET Archives

July 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Genny Gibbard <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Genny Gibbard <[log in to unmask]>
Date:
Mon, 21 Jul 2008 13:10:02 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (63 lines)
 Thanks for posting, Steve.
My concern?  IPC-2221, Table 6-1 minimum electrical conductor spacing.
For a low voltage assembly is 0.13mm.  These solder balls are hugging
one pad, so they aren't a problem.  I probably agree that I wouldn't
fail this particular board.  If this solder ball trapped itself in
between two pads, though, it is like a little stepping stone between the
pads - the space on either side is less than the minimum clearance spec.
Maybe I am applying this incorrectly?


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: July 21, 2008 11:54 AM
To: [log in to unmask]
Subject: Re: [TN] Solder balls

Hi Genny!

Sorry it's taken me a bit to get your picture posted, but I just got
back from 2-weeks vacation and a week in Colorado going to a
IPC-771/7721 instructor certification class, so I've been catching up on
things this morning. But here is your picture:

http://stevezeva.homestead.com/files/solderballs-QFN.jpg

Myself, I wouldn't worry about them tiny solderballs. They probably
aren't going anywhere, and besides if they did, they're so small what
problem could it cause?

Steve

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Monday, July 21, 2008 10:52 AM
To: [log in to unmask]
Subject: [TN] Solder balls

Have you ever gotten a much better analytical tool available to you, and
have it cause major panic due to what you can see now that you never saw
before?
We got a major fancy dancy brand new X-Ray.
Now we see things like the attached picture.  Steve, could I trouble you
to post it for me?  
 <<solderballs-QFN.jpg>>
Our old X-Ray would have never seen this.
Would you fail these solder balls?

It is a QFN, 0.5mm pitch, 0.3mm pad width with a heat slug.
I think trying to replace this device by hand would cause more trouble
than we see right now.

Genny 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2