TECHNET Archives

November 2005

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
David Greig <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, David Greig <[log in to unmask]>
Date:
Fri, 11 Nov 2005 18:45:59 -0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (59 lines)
Glass filled PES(polyethersulphone), and PEI(polyetherimide) and PSF(polysulphone) are used in burn in sockets upto ~170C

Pretty sure the first 2 are machineable.

Best Regards

David Greig
______________________________
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
t: +44 (0)1383 624 975
www.gigadyne.co.uk
______________________________

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Tremmel
Sent: 11 November 2005 18:20
To: [log in to unmask]
Subject: [TN] High temp material

Hello all,

Would anyone recommend a high-temp material that can:

Be machined for various fixtures and chucks Can withstand lead-free oven profiles Be used for 100 or more thermal cycles and
still maintain its form (down to 1mil tolerance) Does not absorb too much heat (compared to a metal)


Thank you in advance,

David

_________________________________________________________________
MSN Latino: el sitio MSN para los hispanos en EE.UU. http://latino.msn.com/

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with
following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send
e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC
web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at
[log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2