TECHNET Archives

November 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Evan D Jones <[log in to unmask]>
Date:
Tue, 17 Nov 1998 11:05:35 +1000
Content-type:
text/plain; charset=us-ascii
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Parts/Attachments:
text/plain (94 lines)
Steve,
     It's  a little hard to tell from your description, but one possibility
is outgassing. If you've got moisture in the card, coupled with the
possibility of poor through hole plating, the card may be outgassing
causing blow holes which appear  randomly over the card surface. Doing a
bake of the card , with weighing of cards before and after bake, will
verify or eliminate this possibility.

Regards Evan

Evan Jones
Manufacturing/Test Engineer
Bluegum Technology Pty Ltd
PO Box 609, Wangaratta, Australia, 3676
Ph: 61 3 5720 2539     Fax: 61 3 5720 2412
Internet:  [log in to unmask]




"Stephen R. Gregory" <[log in to unmask]> on 17/11/98 09:51:17

Please respond to "TechNet E-Mail Forum." <[log in to unmask]>; Please respond
      to [log in to unmask]

To:   [log in to unmask]
cc:    (bcc: Evan Jones/BGT)
Subject:  [TN] Weird Wave Soldering Defect...




Hi Ya'll!

     I've been wave soldering some boards today that we've been building
for a
customer over the last 2-months. They're a little 2" X 2" PTH board in a
30-up
panel, and haven't given me a lick of trouble till today...been waving fine
for the past two months. Other than wanting to bow big time while warming
up
before hitting the wave, there really isn't much to em'.

      They came out of the wave today with random barrels missing
solder...and
when you look at the barrels that's missing solder, it's like the solder
just
tinned the barrel and lead, and then said "hasta la vista baby, I'm outta
here.." and just dropped outta the holes?!?! It's random too...not
concentrated in any one area. What's got me perplexed is why did it appear
that it wet to the barrel and lead by the way it tinned them, but didn't
stay
up in the barrel? There's no vibration anywhere, and the conveyer runs as
smooth as a babies butt...and I don't use a hot air knife.

       Nothing has changed with my settings that I've used over the past
2-months and have been working great up until today. I'm water soluble,
foam
stone fluxer, Soltec Prisma with convection pre-heat, and Kester Flux.
Cleaned
the pot and flux tank this weekend, so I was starting with a nice
dross-less
pot and fresh flux...so what gives? Anybody seen this before? Any ideas?

Thanks in Advance!

-Steve Gregory-

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2