Bill,
I get the same results as shown.
R = (100/2 + 35) * [(100-.3)/.3] - 75 = 28173 um
Ben
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Byrd, Bill J
Sent: Tuesday, June 02, 2015 1:34 PM
To: [log in to unmask]
Subject: EXTERNAL: [TN] minimum flex bend radius
Hello,
IPC-2223 contains an equation labeled 'Equation 2' for calculating the minimum bend radius for double-sided circuits with coverlay. I wonder if I am missing something because when I plug in the values shown there as an example the 'R' value does not match what is shown there. Any help would be appreciated.
Bill
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|