TECHNET Archives

March 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 29 Mar 2013 09:27:34 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Guy Ramsey <[log in to unmask]>
Message-ID:
<00f501ce2c81$2d0d9030$8728b090$@com>
Subject:
From:
Guy Ramsey <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (38 lines)
Background info: 
We were asked to populate and assembly with a Ma-Com part, MA46H120, a GaAs
Constant Gamma Flip-Chip Varactor Diode. The data sheet says: 

Mounting Techniques - These chips were designed to be inserted onto hard or
soft substrates with the junction side down. They can be mounted with
conductive epoxy or with a low temperature solder preform. The die can also
be assembled with the junction side up, and wire or ribbon bonds made to the
pads.

Solder Die Attachment - Solder which does not scavenge gold, such as
Indalloy #2 (80In-15Pb-5Ag) is recommended. Sn-Pb based solders are not
recommended due to solder Embrittlement.  Do not expose die to a temperature
greater than 235C, or greater than 200C for longer than 10 seconds.

The Indalloy #2 cost $2,222.00 for 100gm or type five solder paste. 

We now have another customer asking for us to solder to thick gold. They
don't have a low temp requirement and asked for SnAu solder (Indalloy #182)
80Au-20Sn. . . I shudder to think what that will cost, and I don't think the
part, an inductor, will survive the 300C reflow. 

Question: 
Does SAC 305 "scavenge gold"? Would it form a brittle solder connection on a
thick soft gold pad? 

Guy






______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2