TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Bev Christian <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Sat, 28 Mar 1998 23:25:58 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (58 lines)
Eddie,
We have had no problems with this finish, after the usual teething problems
and some inspector education.  However, I would suggest that you see how it
works with other fluxes.  Solder joints with this finsh are definitely flux
dependent.

Bev Christian
Nortel

> ----------
> From:         Eddie Brunker[SMTP:[log in to unmask]]
> Sent:         Friday, March 27, 1998 5:50 AM
> To:   [log in to unmask]
> Subject:      [TN] Parts Solderability (2)
>
> Hi,
>
> What about the solderability of Palladium finished leads on TI devices.
> I'm
> surprised this subject hasn't been discussed on this list! TI are
> determined
> to continue with their lead free technology in spite of the fact that it
> doesn't work. Palladium just isn't a highly solderable finish. In spite of
> numerous companies finding problems with these devices, it fails to get
> discussed! There is a white paper on a TI web site which proclaims the
> virtues of this finish. It would make a very interesting basis for a
> thread
> of discussion. http://www.ti.com/sc/docs/asl/palladm
>
> Regards,
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
> information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2