We recycle any scrap we have, also, our customers send us on occasion their
scrapped product for recycling...
During this recycling, the solder (Sn/Pb) coating is stripped off, I think
they try to reclaim the copper as well, and the laminate and mask are made
inert then sent to a company that makes industrial fuel out of the...mess...
The cost to have this "disposed "of" this manner is offset by the
reclaim/recovery cost (tin lead and gold) so we're usually not out any
money...maybe a few buscks here and there.
Also, saves on tons of TNRCC and EPA paperwork...
Franklin
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|