TECHNET Archives

May 2009

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Hernefjord Ingemar <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Hernefjord Ingemar <[log in to unmask]>
Date:
Tue, 26 May 2009 09:00:49 +0200
Content-Type:
text/plain
Parts/Attachments:
text/plain (95 lines)
It's sad that one country prefered to demonstrate the opposite. 
/Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bernard Kessler
Sent: tisdag 26 maj 2009 01:32
To: [log in to unmask]
Subject: Re: [TN] Memorial Day

Hi---
In the context of your exchange --- Bev and Steve ---- Memorial Day 1952 I was an Army officer living on a Naval ship as part of a convoy bringing men and material to St. Anthony, Newfoundland to build a radar station as part of the DEW line --- the Distant Early Warning system --- built up in the cold war.  Then, too, we paused for a brief minute to remember those we served with in WWII and wondered when and where the next encounter may take place.  That operation --- our part --- was a joint US-Canadian project.  Many memories.
Best to all
Bernie Kessler


At 03:52 PM 5/25/2009, stephengregory5849 wrote:
>I am. I want to say that I also contemplate Canada's losses from war. 
>Your nation has also given it's treasure for the same...
>
>One of my fondest memories from my Navy days was participating in a 
>yearly joint exercise that was hosted by our Canadian friends out of 
>RCAF Comox on Vancouver island. What great times! I still have the RCAF 
>patch I was able to get from over 30-years ago.
>
>Steve
>
>----- Original Message ----- From: "Bev Christian" <[log in to unmask]>
>To: <[log in to unmask]>
>Sent: Monday, May 25, 2009 3:56 PM
>Subject: [TN] Memorial Day
>
>
>We hope our American friends are having a pleasant long weekend and are 
>spending at least a few minutes contemplating the losses that make 
>"life, liberty and the pursuit of happiness" possible.
>
>Bev
>RIM
>The Great White North
>
>
>---------------------------------------------------------------------
>This transmission (including any attachments) may contain confidential 
>information, privileged material (including material protected by the 
>solicitor-client or other applicable privileges), or constitute 
>non-public information. Any use of this information by anyone other 
>than the intended recipient is prohibited. If you have received this 
>transmission in error, please immediately reply to the sender and 
>delete this information from your system. Use, dissemination, 
>distribution, or reproduction of this transmission by unintended 
>recipients is not authorized and may be unlawful.
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
>unsubscribe, send a message to [log in to unmask] with following text in 
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
>or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
>per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: 
>http://listserv.ipc.org/archives Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
>unsubscribe, send a message to [log in to unmask] with following text in 
>the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
>or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
>per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: 
>http://listserv.ipc.org/archives Please visit IPC web site
>http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
>information, or contact Keach Sasamori at [log in to unmask] or 
>847-615-7100 ext.2815
>-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2