Ioan,

When we built Lead Free hardware for our internal and several external
trials, we used the same stencils as we would for SnPb and found not
problems with them. In fact, several of our technicians found Lead Free
solder paste to be easier to print than their SnPb counterparts.

While I doubt that the rheology of Lead Free and SnPb solder pastes are
identical, based on our experience, they are close enough to work
without changing the screen printing process parameters.

Hope this helps. Give me a call off-line for additional details.

Good Luck.

Lee Whiteman
Senior Manufacturing Engineer
ACI
E-Mail: [log in to unmask] <mailto:[log in to unmask]>
Ph: (610) 362-1200 x208
Fax: (610) 362-1290



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Tempea,
Ioan
Sent: Wednesday, June 11, 2003 7:40 PM
To: [log in to unmask]
Subject: [TN] Stencils for Pb-free


Hi Technos,

since there are not so many takers for Sasha's problems, I wonder if I
could tease you some more.

OK, there will be issues with material control, duplicate BOMs and AVLs,
removable solder pots, etc. But, what about the stencils? Will I be able
to use the stencils I use right now, or they are too contaminated with
Pb? Is the rheology of the PB-free paste identical to the one of the
SnPb? Should I keep the homeplating, or the full apertures will be OK?

Thanks,
Ioan

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2