Hi!
There are many problems with thermal mismatch and mechanical handling , as
all our friends have mentioned. The first nono I know, if you dare to ignore
them, is -don't put the large ones through wave soldering. Most chip
capacitor manufacturers give charts in their catalogs , in which you can see
if your choice of capacitor is good according to your process. They give you
also reflow profiles , pad size, a.s.o.
I don't want to play the all knowing person to you. We had the same problems
and changed component size, designs, handling procedures.
Good Luck!
Gaby
> ----------
> From: Wanner Bernhard[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;Wanner Bernhard
> Sent: ?יום רביעי 10 נובמבר 1999? 18:57
> To: [log in to unmask]
> Subject: [TN] 1812 capacitors on FR-4
>
> -----Ursprungliche Nachricht-----
> Von: Matthew Lamkin
> [SMTP:[log in to unmask]]
> Gesendet am: Freitag, 25. Juni 1999 09:26
> An: [log in to unmask]
> Betreff: Re: [TN] FW: What it would be like living in
> Australia
>
> Well I don't know about being a joke, but I've saved it as a handy
> little utility.
> By selecting it from my start menu I can now turn a PCB that I am
> working on upside down to view it from another angle.
>
> Something that I have occasionally wanted to do. I can remember
> actually
> going as far as turning the monitor on its side
> before, just so that I could view something from a different angle
> without upsetting everything else in the PCB file.... <g>
> Hi technos, we have some problems with 1812 (and also with 1210)
> capacitors
> on FR4 because cracks at the corner. Is there any size limit for SMT cap's
> on FR4 (may be different classed for different application temperatures)?
> Thanks, Bernhard, Zurich
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in
> the body:
> To subscribe: SUBSCRIBE TECHNET <your full name>
> To unsubscribe: SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################
>
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|