Use the same process as any other SMT process with a few Precautions.
1) BGA are very susceptible to moisture, bake them if they have been exposed.
2) Inspect Solder paste before placement, 100% (this is normally the biggest
gotcha)
3) If placement is off, do not attempt to "tweak" the part, remove clean board
and part and reapply solder paste.
4) Profile with a thermocouple attached to the solder ball, (drill a small
hole through the board and feed the wire from the bottom (a ball closet to the
middle is best)
Hope this helps
Mike
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|