Message-ID:
<2102A6E85EAF4978A3EDCD9641B4B7CB@stephenPC>
Subject:
From:
Steve Gregory <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; format=flowed; charset="utf-8"; reply-type=original
MIME-Version:
1.0
Parts/Attachments:
text/plain (97 lines)
Direct from the manufacturer...

Steve

-----Original Message----- 
From: Joyce Koo
Sent: Wednesday, February 22, 2012 8:50 PM
To: [log in to unmask]
Subject: Re: [TN] Air Bubbles in Syringes of Solder Paste...

Did you get directly from mfg or ask distributor to re package it for you?
--------------------------
Sent using BlackBerry


----- Original Message -----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Wednesday, February 22, 2012 07:58 PM
To: [log in to unmask] <[log in to unmask]>
Subject: Re: [TN] Air Bubbles in Syringes of Solder Paste...

I meant to say 35-gram syringes...

Steve

From: Steve Gregory
Sent: Wednesday, February 22, 2012 7:51 PM
To: [log in to unmask]
Subject: [TN] Air Bubbles in Syringes of Solder Paste...

Hi All,

I have a question about syringes of dispensable solder paste. We purchase 
10cc syringes of Type-4 dispensable solder paste for work that we do. It’s 
used much of the time to dispense paste for the stacked capacitors that we 
do, much of the time it’s for 0402 caps, so the dispensing has to be very 
precise.

Recently our operators have complained about the paste, they said they’re 
having a hard time being consistent with the dots they’re trying to 
dispense. One of the operators showed me the syringe that she was using, and 
I was surprised at the air bubbles I saw inside the syringe. The photos 
below are pictures I took under a microscope through the side of the 
syringe:

http://stevezeva.homestead.com/AirBubbles.jpg

http://stevezeva.homestead.com/AirBubblesClose.jpg

I can see why she was having trouble. As I said, we buy these syringes 
pre-filled, they come to us packaged in a cool pack, and we store them 
immediately in the refrigerator until they are ready to be used. They are 
taken out and allowed to come up to room temperature before they are ever 
attached to a dispenser. We use EFD dispensers BTW.

I looked at the syringes that were un-touched and stored in the 
refrigerator, and they had the same sort of bubbles. So our dispensers are 
not introducing them, and it seemed like the bubbles were only associated 
with one lot of of syringes. There was another lot in the refrigerator that 
did not have the bubbles.

So my question is (not being a solder paste vendor), how are these syringes 
filled ? Do they centrifuge them to eliminate the bubbles ? I know I did 
that in the past when I filled syringes with chip bonder for our Fuji 
dispenser, in fact, the centrifuge was sold to us by Fuji. But I’m not sure 
about solder paste. How do you go about making sure there are no bubbles in 
syringes of solder paste ? Is there anything we can do with the paste that 
we have to eliminate the bubbles or should we just send the paste back ?

Steve

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from your 
system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________ 


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2