To Jon,
I sent a mail to you with wrong value. I wrote '5,000 V/micrometer' for best
Kapton tape. Well, that would been a dream for people doing with high
voltage applications.
The correct value is 50 V/micrometer. There are some application with higher
dielectric withstanding, e.g. in semiconductors. We design certain HBT and
MESFETs for withstanding over 100 V/micrometer, but it's not applicable in
your case, I believe.
/Inge
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|