quoted-printable
Content-Type:
text/plain; charset="UTF-8"
From:
Werner Engelmaier /* <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
Hi Neil,
No such standard exists or can exist, because [drum roll]—'It depends!'
It depends on thicknees of the layers [each one individually], the modulus of 
elasticity [of each layer—from this the location of the neutral plane is 
determined], and the ductility of each metallic layer [use IPC-TM-650, 2.4.2.1 
"Flexural Fatigue and Ductility, Foil,” or ASTM   E 796 “Standard Test Method 
for Ductility Testing of Metallic Foil”].
Having all of this, you can determine the minimum sustainable bend radius.
You can find the methodology in IPC-D-330, Section 6.2.1.2 “Flexibility 
Considerations in the Design of Flexible Printed Wiring”   [most likely 
out-of-print] or in the upcoming book by Joseph Fjelstad Flexible Circuit Technology, 4th 
edition.

Werner
Future workshops:
Reliability Issues with Lead-Free Soldering Processes, June 17, London
Interconnect Failures and Design for Reliability for PCB PTHs, June 17, 
London
Pb-Free Soldering Processes—Survival, Quality, Reliability, August 18, 
Orlando
Reliability Issues with Lead-Free Soldering Processes, September 22, 
Schaumburg
Failure Mode and Root Cause Analyses Reliability (Fatigue, Brittle Fracture, 
ENIG), September 22, Schaumburg



**************
Wondering what's for Dinner Tonight? Get new twists on family 
favorites at AOL Food.
      
(http://food.aol.com/dinner-tonight?NCID=aolfod00030000000001)

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2