In a past life we used them in MIL application. Put them on Kevlar PCB's to provide a better CTE match. Limited size (I believe it was LCC20 or LCC24 max...). Also used elevated solder joints.
Bottom line... Was a very costly part to use (material $ for PCB, process development and validation, special process, etc.)
Also used them mounted to a ceramic substrate. Perfect CTE match, no problems.
>>> [log in to unmask] 07/20/00 11:35AM >>>
Greetings,
Is anybody out there using leadless ceramic chip carriers in a military environment without attaching leads? If so, what size are you using?
Thanks in advance for any information,
Bill Robinson
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|