Steve,
If this was a print and etch job like inner layers I would be saying "holy
resist failure Batman" and would have suspected that your suppliers resist
had a run of bubbles or loss of adhesion areas as some of the failures are
called "etch downs". Since the resist on an outer layer is the tin lead or
tin then one has to suspect that some contaminant, usually resist residue,
prevented the plating. Interesting that etch out areas are so round, still
looks like bubbles. Rudy, Hydrogen evolution or bubbles?
Chuck
-----Original Message-----
From: Stephen Gregory [mailto:[log in to unmask]]
Sent: Tuesday, April 05, 2005 6:45 AM
To: [log in to unmask]
Subject: [TN] Mousebites...
Mornin' all ya'll!
Came back in this morning and looked at the fabs that I posted about
yesterday some more. We're going to reject them.
Not just because of the mousebites on the annular pads, but we've
discovered that there are mousebites all over everything. In some
cases reducing the trace widths.
Take a look at; "Mousebites 1-4" at: http://www.stevezeva.homestead.com
If it were just the annular pads, we might have accepted them. But not with
them occuring all over the fab like this.
Kind regards,
-Steve Gregory-
Senior Process Engineer
LaBarge Incorporated
Tulsa, Oklahoma
(918) 459-2285
(918) 459-2350 FAX
__________________________________________________________________
This message may contain information that is privileged and confidential to
LaBarge, Inc. It is for use only by the individual or entity named above.
If you are not the intended recipient, you may not copy, use or deliver
this message to anyone. In such event, you should destroy the message and
kindly notify the sender by reply e-mail.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|