Ron Hayashi wrote:-
>Is anyone experiencing debris in the holes after drill and/or debris in the
>flute of the drills? We seem to find it more prevalent on high layer
>count/resin rich constructions.
Hi Ron,
Assuming good quality drills, good extraction, and the correct
feed/speed parameters, it may be you are trying to drill too high a
stack. If that is the case, then peck drilling will eliminate the
problem. One peck half way down with the second all the way through may
be sufficient, or perhaps three pecks.
If you cannot peck drill, then try reducing the stack height.
Merry Christmas,
Paul Gould
[log in to unmask]
Teknacron Circuits Ltd
Isle of Wight,UK
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|