I believe that this is decimeter. So .6 would be 6ASF
Scott Westheimer
----- Original Message -----
From: "Roby D Hott" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, January 29, 2004 2:13 PM
Subject: [TN] current density
> Greetings from snowy Indiana -
>
> We are in the process of reviewing all of the test methods associated with
> IPC-6012 in an effort to have them updated, if necessary, with the release
of
> IPC-6012B.
>
> In Method 2.3.15 Purity of Copper Foil or Plating there is a para as
follows:
> 4.3.5 Current source capable of supplying a current density based on the
> cathode area of at least 0.6A/dm(2).
>
> I don't know what "d" or "m" stand for in this formula.
>
> Can any of you help?
>
> Susan Mansilla
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------