TECHNET Archives

January 2008

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Whittaker, Dewey (EHCOE)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Whittaker, Dewey (EHCOE)
Date:
Wed, 30 Jan 2008 07:00:41 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (203 lines)
Steve,
Graham made some excellent points and I agree with everything he said
except we've bent a few lights with him in the past (Miller, of course).
Speaking of good taste; you can't go wrong taking advice from Graham,
unless it's about Rugby shirts, then I'd get a second opinion.
Dewey

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
Sent: Wednesday, January 30, 2008 6:04 AM
To: [log in to unmask]
Subject: Re: [TN] Humiseal UV40 Conformal Coating

Hi Steve

My apologies for this tardy reply - just bought another business which  
kept me rather busy.

In answer to your question, take care.

UV curables offer superb fast cure in seconds - on 2D objects. The  
tough part is getting the coating to cure where the light doesn't  
shine, and it is really tough to bend light!

All UV's need to use a secondary cure mechanism to facilitate curing  
in shadow areas. Often this is a moisture cure, but often it fails to  
cure off for anything up to 7 days. Furthermore the product is  
ionically "active" until it has cured.

Most of these issues have been addressed in UV40, but how fast you can  
put the end product in a box to ship is something you should check for  
yourself. The last thing you need is for the coating to flow out from  
underneath components whilst in transit.

A comment if I may: Changing the coating to get the product out of the  
door is not the sort of design brief I would feel comfortable with. A  
full product re-qualification would be required.

Back to the coating you do use: Most urethanes are moisture cure  
unless you are working with 1A33? If it is 1A33, then you should be  
able to ship sooner than 20 hours.

I would prefer to see the following terms used:

Tack-Free
Dry
Fully cured

You can get most urethane coatings Dry - no flow-out during transit -  
within around 8 hours or less.

Let me know which coating you use and I might be able to suggest an  
alternative schedule.

Graham

Gen3 Systems
www.gen3systems.com - Engineering Reliability in Electronics

On 25 Jan 2008, at 18:39, Steve Gregory wrote:

> Hi Graham!
>
> It's funny that this thread should come up now. We just realized that
> the urethane coating we use requires at least a 20-hour cure, and
> everybody went into a tizzy about our ship schedule.
>
> I was then asked if I knew anything about UV cure coatings, which I
> don't. So my first question is; how long does it need to cure before
> it's ready to ship? I understand that it might not be fully cured and
> ready for full service, but rarely, if ever, do we ship something to  
> our
> customer that will get put into full service as soon as the they  
> receive
> it.
>
> Also, what kind of UV source, or oven would you recommend?
>
> Thanks!
>
> Steve Gregory
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
> Sent: Friday, January 25, 2008 11:55 AM
> To: [log in to unmask]
> Subject: Re: [TN] Humiseal UV40 Conformal Coating
>
> Amol
>
> It is indeed a new coating, and a good one. There are several users in
> Europe who, not speaking English, don't see the Technet. What do you
> need to know and I will see if I can help
>
> Kindest regards
>
> Graham Naisbitt
>
> Work:  [log in to unmask]
> Home: [log in to unmask]
>
>
>
>
> On 23 Jan 2008, at 12:41, Kane, Amol (349) wrote:
>
>> Dear TechNetters,
>> Does anybody have any Experience (good or bad) with Humiseal's UV40
>> Conformal Coating?......we will need to use it on some of our boards
>> soon and just wanted to test the waters to see if anybody else is
>> already using it.
>>
>> We already do UV cure coatings and have the necessary setup.
>>
>> Thanks in advance,
>> Amol
>>
>>
>>
>>
>> WARNING:  Export Control
>> This document may contain technical data within the definition of the
>> International Traffic in Arms Regulations (ITAR), and subject to the
>> Export Control Laws of the U.S. Government.  Transfer of such data by
>> any means to a foreign person, whether in the United States or  
>> abroad,
>
>> without proper export authorization or other approval from the U.S.
>> Department of State is prohibited.
>>
>> CONFIDENTIALITY NOTICE:
>> This e-mail, and any attachments, is for the sole use of the intended
>> recipient(s) and may contain information that is confidential and
>> protected from disclosure under the law. Any unauthorized review,  
>> use,
>
>> disclosure, or distribution is prohibited. If you are not the  
>> intended
>
>> recipient, please contact the sender by reply e-mail, and delete/
>> destroy all copies of the original message and attachments.
>> Thank you.
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
>> unsubscribe, send a message to [log in to unmask] with following text  
>> in
>
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
>> or (re-start) delivery of Technet send e-mail to [log in to unmask]
>> : SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]
>> : SET Technet Digest
>> Search the archives of previous posts at:
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at
>> [log in to unmask]  or 847-615-7100 ext.2815
>> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily  
> halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16  
> for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2