Have you considered a stepped stencil to provide greater paste volume around the component requiring IR?
>>> [log in to unmask] 04/11/03 09:22AM >>>
Have you tried oblong apertures? As far as I know, studies made showed
overprint of something like 125 mils didn't cause solder balls.
-----Original Message-----
From: Tempea, Ioan [mailto:[log in to unmask]]
Sent: Friday, April 11, 2003 5:22 AM
To: [log in to unmask]
Subject: [TN] Apertures for intrusive reflow
Hi Technos,
I am investigating intrusive reflow and big part of the topic is OK for me.
I learned how to calculate the volume of the paste, I even tried the process
on several assemblies, all OK.
Now I'm running into a board with less real estate, so not so much space to
do the overprinting. According to my calculations the apertures for this
particular TH connector would overlap. It's a 78.7 mils pitch.
The question is: could I overlap the apertures and print paste all over,
bridging between the pins? Since we deal with large pitch and we're talking
liquid paste flowing towards the holes, would this not create solder bridges
after reflow?
Thanks for your insights,
Ioan
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
________________________________________________________________________
This email has been scanned for computer viruses.
________________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
This email has been scanned for computer viruses.
|
|
|