We have an assembly that uses tin plated pins and sockets for the
interconnection. We are having trouble getting the pin side in tin but is
readily available in gold. My question is "is there any long term problems
putting a gold pin in a tin plated socket"?
For years people have put I/C leads into gold sockets without problem so it
seems that this should not be a problem but thought I'd ask for any real
life experiences.
Thanks,
Ken Bloomquist
Sr. Principal Process Engineer
PRIMEX Aerospace Company
P.O. Box 97009
Redmond, WA 98073-9709
www.primextech.com
Ph: 425-885-5000
FAX: 425-882-5786
[log in to unmask]
Northcon/98, Show Director
<www.northcon.org>
Electronics Manufacturers Association (EMA), Secretary
<www.ema-wa.org>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|