I'm having a perplexing problem with what appears to be dye staining on
Teflon laminate.
The laminate is 6010 LM Teflon. The stain occurs in the developer, on
exposed Teflon areas. Running the material through a fresh developer
solution eliminates the staining; the problem is I have a number of parts
that are already stained and I need to remove it. I've tried various
cleaners, solvents, and of course, stripper solution. Nothing seems to
affect the stain.
Anyone have any suggestions that will help me remove this stain?
Thanks.
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|